Posts: 7,421
Threads: 1
Joined: Sep 2005
First of all you have to allow for a full cure, which for most finishes I believe is about 200 hours (about 7 days).
I would think a breathable pad would be best. Felt comes to mind. It comes in various colors and in thicknesses up to 1". It has some slip resistance, but it is not in the same class as silicon rubber.
My second choice would be cork. It is a natural product. Some of it is just harvested in sheets. Some of it is made like particle board. I think the natural version would be superior for this purpose.
I don't know where to get it in small quantities.
I put a glass table top on top of 3M "bumpons and I cannot pry the glass off the top. I'm afraid I will shatter it if I pry harder.
https://www.mantoncork.com/cork-products/
No animals were injured or killed in the production of this post.
Posts: 7,421
Threads: 1
Joined: Sep 2005
Consider covering the entire bottom of your piece. It will spread the weight over more square inches and possibly reduce the risk of imprinting. But do wait for a “full cure” before pitting anything on the surface for an extended time.
No animals were injured or killed in the production of this post.
Posts: 6,678
Threads: 1
Joined: Jan 2003
Location: Southern California
LV sells anti-slip material (same as used in woodworking hockey pucks). Free shipping until Tues. Give it a try.
Thanks, Curt
-----------------
"Life can only be understood backwards; but it must be lived forwards."
-- Soren Kierkegaard